Is it good to coat in Dover, DE this week?

A live 7-day go/no-go calendar for epoxy & resin floors in Dover, built from the local forecast against the 5°F-above-dew-point rule. We lead with the signal a weather app misses: overnight condensation risk.

TodayHold offBest upcoming window: Tue (Caution)
SunRISK
79°/71°
Dew margin
-0.2°F
Overnight dew
High
Rain
9%
Window

High condensation risk overnight — surface dips to within -0.2°F of the 68°F dew point (low 66°F, 100% cloud, 2 mph wind). A fresh coat can blush/blister. Stop 4h before dew falls.

MonRISK
82°/70°
Dew margin
0.2°F
Overnight dew
High
Rain
2%
Window

High condensation risk overnight — surface dips to within 0.2°F of the 63°F dew point (low 63°F, 21% cloud, 4 mph wind). A fresh coat can blush/blister. Stop 4h before dew falls.

TueCAUTION
83°/72°
Dew margin
3.7°F
Overnight dew
Watch
Rain
7%
Window
8am–5pm

Watch overnight dew — surface comes within 3.7°F of the dew point (margin is 5°F). Time the coat to dry well before evening.

WedRISK
93°/75°
Dew margin
5°F
Overnight dew
Low
Rain
7%
Window

Too hot — high of 93°F is well over the 86°F ceiling; the film skins over before it can level or adhere.

ThuRISK
97°/81°
Dew margin
8.1°F
Overnight dew
Low
Rain
2%
Window

Too hot — high of 97°F is well over the 86°F ceiling; the film skins over before it can level or adhere.

FriRISK
100°/85°
Dew margin
11°F
Overnight dew
Low
Rain
19%
Window

Too hot — high of 100°F is well over the 86°F ceiling; the film skins over before it can level or adhere.

SatRISK
99°/80°
Dew margin
3.8°F
Overnight dew
Watch
Rain
29%
Window

Too hot — high of 99°F is well over the 86°F ceiling; the film skins over before it can level or adhere.

Hold offSun — today & tonight
  • High condensation risk overnight — surface dips to within -0.2°F of the 68°F dew point (low 66°F, 100% cloud, 2 mph wind). A fresh coat can blush/blister. Stop 4h before dew falls.
  • Rain likely in the 24h cure window (9% chance, ~6.2mm) — it can wash out or mar an uncured coat.
  • High humidity (94%, over the 85% mark) slows drying — keep an eye on the cure window.

Hold off. These are forecast numbers — confirm the surface temperature on-site before you start.

Why these thresholds

Installing within 5°F of the dew point causes amine blush / carbamation — a cloudy, greasy, hazed floor. The slab surface temp, not the air, is what counts.

  • • Surface temp must stay 5°F above the dew point through application and cure (ASTM D3276 / ISO 8502-42).
  • • Air + surface in the 5086°F band (low-temp lines to 50°F).
  • • Humidity under 85%; ideally under 80%.
  • • No rain for 24h after application.
  • • We use the forecast ground-surface temperature as a surface-temp proxy — confirm on-site with an IR thermometer.

Free in the beta

Watch this job site 24/7

Get an email the moment overnight dew, rain, or an out-of-range stretch threatens a fresh coat — and a morning digest with the best window ahead. No app to check; we watch the forecast for you.

Set up a free alert

Other coatings in Dover

Epoxy & Resin Floors weather elsewhere in Delaware