paint·day

Is it good to stain in St. Petersburg, FL this week?

A live 7-day go/no-go calendar for deck & fence stain in St. Petersburg, built from the local forecast against the 5°F-above-dew-point rule. We lead with the signal a weather app misses: overnight condensation risk.

TodayHold offBest upcoming window: Sun (Caution)
FriRISK
90°/77°
Dew margin
0.6°F
Overnight dew
High
Rain
39%
Window
—

High condensation risk overnight — surface dips to within 0.6°F of the 75°F dew point (low 75°F, 100% cloud, 4 mph wind). A fresh stain can blush/blister. Stop 4h before dew falls.

SatRISK
83°/75°
Dew margin
4.7°F
Overnight dew
Watch
Rain
47%
Window
—

Humidity peaks at 98% — well above the 85% ceiling; cure stalls and moisture gets trapped.

SunCAUTION
87°/79°
Dew margin
5.2°F
Overnight dew
Low
Rain
37%
Window
8am–5pm

Some rain risk (37%) during the cure window — re-check the radar before you start.

MonRISK
87°/81°
Dew margin
4°F
Overnight dew
Watch
Rain
68%
Window
—

Rain likely in the 24h cure window (68% chance, ~10.1mm) — it can wash out or mar an uncured stain.

TueRISK
85°/80°
Dew margin
2.6°F
Overnight dew
Watch
Rain
89%
Window
—

Rain likely in the 24h cure window (89% chance, ~7.1mm) — it can wash out or mar an uncured stain.

WedRISK
84°/79°
Dew margin
3.4°F
Overnight dew
Watch
Rain
80%
Window
—

Rain likely in the 24h cure window (80% chance, ~9.2mm) — it can wash out or mar an uncured stain.

ThuRISK
86°/80°
Dew margin
4.4°F
Overnight dew
High
Rain
67%
Window
—

High condensation risk overnight — surface dips to within 4.4°F of the 72°F dew point (low 76°F, 17% cloud, 7 mph wind). A fresh stain can blush/blister. Stop 4h before dew falls.

Hold offFri — today & tonight
  • High condensation risk overnight — surface dips to within 0.6°F of the 75°F dew point (low 75°F, 100% cloud, 4 mph wind). A fresh stain can blush/blister. Stop 4h before dew falls.
  • Rain likely in the 24h cure window (39% chance, ~7mm) — it can wash out or mar an uncured stain.
  • High humidity (91%, over the 85% mark) slows drying — keep an eye on the cure window.

Hold off. These are forecast numbers — confirm the surface temperature on-site before you start.

Why these thresholds

Stain applied to a damp or dew-wet board can't penetrate — it beads, stays tacky and flakes. Wood must be dry and stay above the dew point while it sets.

  • • Surface temp must stay 5°F above the dew point through application and cure (ASTM D3276 / ISO 8502-42).
  • • Air + surface in the 50–90°F band (low-temp lines to 45°F).
  • • Humidity under 85%; ideally under 70%.
  • • No rain for 24h after application.
  • • We use the forecast ground-surface temperature as a surface-temp proxy — confirm on-site with an IR thermometer.

Free in the beta

Watch this job site 24/7

Get an email the moment overnight dew, rain, or an out-of-range stretch threatens a fresh coat — and a morning digest with the best window ahead. No app to check; we watch the forecast for you.

Set up a free alert→

Other coatings in St. Petersburg

Deck & Fence Stain weather elsewhere in Florida